- News
- Books
Featured Books
- pcb007 Magazine
Latest Issues
Current IssueThe Growing Industry
In this issue of PCB007 Magazine, we talk with leading economic experts, advocacy specialists in Washington, D.C., and PCB company leadership to get a well-rounded picture of what’s happening in the industry today. Don’t miss it.
The Sustainability Issue
Sustainability is one of the most widely used terms in business today, especially for electronics and manufacturing but what does it mean to you? We explore the environmental, business, and economic impacts.
The Fabricator’s Guide to IPC APEX EXPO
This issue previews many of the important events taking place at this year's show and highlights some changes and opportunities. So, buckle up. We are counting down to IPC APEX EXPO 2024.
- Articles
- Columns
Search Console
- Links
- Events
||| MENU - pcb007 Magazine
Estimated reading time: 1 minute
Contact Columnist Form
Dry Film Photoresist Thickness Selection Criteria
Dry film photoresist suppliers typically indicate for which process (e.g., print and etch, pattern plate, tent and etch, gold plating) a certain resist type is suitable; however the fabricator still has to select the resist thickness that matches his needs best. The most important thickness selection criteria that come to mind are price, resolution, and yield.
Dry film photoresist with a thinner photo-sensitive layer tend to have a lower price because of the lower material cost of the resist layer. So it makes sense to use the thinnest resist that still satisfies yield and resolution expectations.
For print and etch, one would choose the thinnest film that still gives acceptable yields. The thinnest resist will also give the best resolution in print and etch because of the more favorable etch channel aspect ratio that will give the best etch factor. The etch channel aspect ratio is defined as the ratio of the total thickness of the resist and the copper to be etched, over the width of the space to be etched. The etch factor is the ratio of vertical etching over lateral etching whereby a high number is more favorable for resolution. High etch channel aspect ratios will result in poorer etch factors. Therefore thinner resist (and thinner copper) give better resolution.
Editor's Note: This article originally appeared in the July 2015 issue of The PCB Magazine.
More Columns from Karl's Tech Talk
Karl's Tech Talk: Digital Imaging UpdateKarl’s Tech Talk: Electronic Packaging Levels
Green Legislation and the Impact on Electronic Materials and Processes
Digital Imaging Revisited
Quick-Turn Circuit Board Shops
Optical Interconnects
Signal Loss
Karl's Tech Talk: Miniaturization and Reliability